Thermal Properties | Metric | English | Comments |
---|---|---|---|
Maximum Service Temperature, Air | 147 °C | 297 °F | for 50% loss of tensile strength after 5000hr |
BASF Ultramid® A3W PA66 (Conditioned) Description: Free-flowing, heat aging resistant and rapidly processable grade for technical parts subject to high stress such as bearings and bearing cages, gearwheels and spool bodies.Information p.. |