Thermal Properties | Metric | English | Comments |
---|---|---|---|
Maximum Service Temperature, Air | 788 °C | 1450 °F | Continuous use |
Pyrotek Pyrotherm M-68 Structural Insulation Board Pyrotherm M-68 is a calcium-silicate board designed for non-ferrous applications. M-68 offers a unique combination of low shrinkage, low thermal conductivity and non-wetting properties which make i.. |
|||
Maximum Service Temperature, Air | 788 °C | 1450 °F | Upper limit of working range |
Heatbath/Park Aluminum Casting Salt AC Aluminum Casting Salt Salt cores can be made with varying melting points to meet the needs of customers who gravity cast as well as those using state-of-the-art die casting machines. Advantages of salt cores over sand c.. |
|||
Maximum Service Temperature, Air | 788 °C | 1450 °F | Continuous |
Aremco Aremco-Seal™ 617 High Temperature Specialty Coatings Glass Glass coating for producing hermetic seals in porous ceramics and refractories to 1450 ºF. Used for sealing high vacuum components, resistance temperature devices, and other electrical sensors. |