Polymer Property : Maximum Service Temperature, Air = 1430 °C Product List

Thermal Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Thermal Properties Metric English Comments
Maximum Service Temperature, Air 1430 °C
2600 °F
Cotronics Resbond™ 901 High Temperature Ceramic Adhesive, Fiber Base
Single component system with a paint consistency.
Maximum Service Temperature, Air 1430 °C
2610 °F
Chosun Refractories 1400BULK Bulk
Information provided by Chosun Refractories via Korea Institute of Ceramic Engineering and Technology (KICET).
Maximum Service Temperature, Air 1430 °C
2610 °F
Chosun Refractories 1400BOARD Board
Information provided by Chosun Refractories via Korea Institute of Ceramic Engineering and Technology (KICET).
Maximum Service Temperature, Air 1430 °C
2600 °F
Continuous
Aremco Cerama-Dip™ 538-N High Temperature Specialty Ceramic-Inorganic Coating
Low viscosity, light gray coating for powder resistors and rheostats to 2600°F (1427°C). black and green pigments also available.
Maximum Service Temperature, Air 1430 °C
2600 °F
Continuous
Aremco Cerama-Dip™ 538-N-BLK High Temperature Specialty Ceramic-Inorganic Coating
Low viscosity, light gray coating for powder resistors and rheostats to 2600°F (1427°C). black and green pigments also available.