Polymer Property : Maximum Service Temperature, Air = 135 °F Product List

Thermal Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Thermal Properties Metric English Comments
Maximum Service Temperature, Air 57.2 °C
135 °F
Saint-Gobain Tygon® 2001 Plasticizer Free Tubing Formulation
Description: Tygon® 2001: Tygon® Plasticizer Free Tubing is a uniquely engineered product that offers the low compression set properties of a thermoset rubber. Tygon® Plasticizer Free Tub..