Thermal Properties Metric English Comments
Maximum Service Temperature, Air 1270 °C
2320 °F
Gouda Vuurvast CURON 127 S Dense Refractory Castable
Description: Curon 127 S castable is characterized by a very high strength and a good resistance against slag attack. This castable is applied mainly in boilers and incinerators.Remarks: These value..
Maximum Service Temperature, Air 1270 °C
2320 °F
Gouda Vuurvast CURON 127 S GM Dense Refractory Castable
Description: Curon 127 S GM gunning castable is characterized by a reasonable strength and a good resistance against slag attack. This castable is applied mainly in boilers and incinerators.Remarks:..