Thermal Properties | Metric | English | Comments |
---|---|---|---|
Maximum Service Temperature, Air | 126 °C | 259 °F | |
Abatron 810328 A/B Filled Potting Compound
(discontinued **) Gray or colors filled casting, potting, adhesive, and coating. Arc track resistant, heavy duty dielectric. 100/17.6 ratio.Information provided by Abatron. |
|||
Maximum Service Temperature, Air | 126 °C | 259 °F | Deflection Temp at unknown load |
Abatron AboCast 8103-28 High-Performance Dielectric Epoxy AboCast 8103-28 is a dielectric in/outdoor epoxy system with superior arc-track resistance, high voltage and heat resistance, low ash and ion content, and it is chlorine-free. This system has high h.. |