Thermal Properties | Metric | English | Comments |
---|---|---|---|
Maximum Service Temperature, Air | 124 °C | 255 °F | |
ConocoPhillips EP Conolith® Grease NLGI NO. 1 Description: Conoco EP Conolith Grease is a high-quality, multipurpose, extreme pressure lithium grease recommended for heavy-duty, heavily loaded antifriction and plain bearings. It is ideal for th.. |
|||
Maximum Service Temperature, Air | 124 °C | 255 °F | Temperature Index |
AlphaGary Megolon™ S500 Low Smoke Halogen Free Sheathing compound allowing significantly improved processing speeds plus good mechanical properties. Application examples include Special Fire Survival / Power Low Voltage / Power Medium Voltage. |
|||
Maximum Service Temperature, Air | 124 °C | 255 °F | Temperature Index |
AlphaGary Megolon™ S501 Low Smoke Halogen Free Sheathing compound allowing significantly improved processing speeds plus good mechanical properties which conforms to BS7655:Section 6.1 Types LTS1 & LTS3 (UK). Application examples include Special.. |