Thermal Properties | Metric | English | Comments |
---|---|---|---|
Maximum Service Temperature, Inert | 149 - 232 °C | 300 - 450 °F | Average value: 226 °C Grade Count:92 |
Overview of materials for Silicone, Molded, Glass Fiber Filled This property data is a summary of similar materials in the MatWeb database for the category "Silicone, Molded, Glass Fiber Filled". Each property range of values reported is minimum and maximum val.. |