Polymer Property : Maximum Service Temperature, Inert = 2910 °F Product List

Thermal Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Thermal Properties Metric English Comments
Maximum Service Temperature, Inert 1600 °C
2910 °F
Inert/Vacuum
Momentive Performance Materials BNC1 Boron Nitride (BN) Refractory Composite
Boron Nitride is a unique engineering material. It is a soft, machinable ceramic which can be combined with other refractory ceramics including Aluminum Oxide, Silicon Nitride, Aluminum Nitride, Mu..
Maximum Service Temperature, Inert 1600 °C
2910 °F
CeramTec SL 200 BG Silicon Nitride, Si3N4-Y2O3
SL 200 BG is a silicon nitride ceramic used to make welding rollers, pins, and components, gas nozzles, and forming tools. Silicon nitrides are ideal for components working under mechanical loads an..
Maximum Service Temperature, Inert 1600 °C
2910 °F
CeramTec SL 200 ST Silicon Nitride, Si3N4-Y2O3
SL 200 ST is a silicon nitride ceramic especially suitable for components exposed to mechanical stress and engine-specific applications even at elevated temperatures. It is recognized for its high s..
Maximum Service Temperature, Inert 1600 °C
2910 °F
CeramTec SL 303 Silicon Nitride, SiAION+SiC
SL 303 is a silicon nitride ceramic. Silicon nitrides are ideal for components working under mechanical loads and engine parts, even and especially at elevated temperatures. Their property profile i..
Maximum Service Temperature, Inert 1600 °C
2910 °F
COI Ceramics SiC Hollow Spheres
Description: COI Ceramics, Inc. can fabricate a variety of thin shell hollow spheres of various compositions and sizes. These products are called Holospheres. They are available as loose spheres tha..