Thermal Properties | Metric | English | Comments |
---|---|---|---|
Maximum Service Temperature, Inert | 1300 °C | 2370 °F | |
CeramTec B 601 Alumina, 98.5% Aluminas exhibit good mechanical properties such as hardness, compressive and tensile strength, and elastic modulus. They perform well at elevated temperatures. |
|||
Maximum Service Temperature, Inert | 1300 °C | 2370 °F | |
CeramTec Rubalit® IS 95 Alumina Rubalit® IS 95 is a high-performance alumina ceramic. Aluminas exhibit good mechanical properties such as hardness, compressive and tensile strength, and elastic modulus. They perform well at eleva.. |
|||
Maximum Service Temperature, Inert | 1300 °C | 2370 °F | |
CeramTec Rubalit® IS 95 Brown Alumina Rubalit® IS 95 brown is a high-performance alumina ceramic. Aluminas exhibit good mechanical properties such as hardness, compressive and tensile strength, and elastic modulus. They perform well at.. |