Thermal Properties | Metric | English | Comments |
---|---|---|---|
Maximum Service Temperature, Inert | 2000 - 3000 °C | 3630 - 5430 °F | Inert/Vacuum Use (BN Component) |
Momentive Performance Materials Boron Nitride (BN) Spray BN aerosol spray delivers high purity, extremely fine, BN crystals in a fast drying solvent-base carrier. It produces a smooth coating with even film build that is virtually binderless.Uses of GE A.. |
|||
Maximum Service Temperature, Inert | 2000 - 3000 °C | 3630 - 5430 °F | Inert/Vacuum Use (BN Component) |
Momentive Performance Materials EPC Boron Nitride (BN) Water Based Coating Solids content > 9%. Can be applied by brush, roller, dipping, or spraying. Can be applied to either hot or cold services although use of water based coatings on surfaces greater than 100°C is .. |
|||
Maximum Service Temperature, Inert | 2000 - 3000 °C | 3630 - 5430 °F | Inert/Vacuum |
Momentive Performance Materials HBC Hot-Pressed Boron Nitride Hot-pressed BN is compacted at temperatures up to 2000°C and pressures up to 2000 psi to form a dense, strong engineering material that is easily machined. It is available in standard and custom.. |
|||
Maximum Service Temperature, Inert | 2000 - 3000 °C | 3630 - 5430 °F | Inert/Vacuum |
Momentive Performance Materials HBT Hot-Pressed Boron Nitride Hot-pressed BN is compacted at temperatures up to 2000°C and pressures up to 2000 psi to form a dense, strong engineering material that is easily machined. It is available in standard and custom.. |
|||
Maximum Service Temperature, Inert | 2000 - 3000 °C | 3630 - 5430 °F | Inert/Vacuum Use (BN Component) |
Momentive Performance Materials HPC Boron Nitride (BN)/TiO2 Water Based Coating Solids content > 25%. Can be applied by brush, roller, dipping, or spraying. Can be applied to either hot or cold services although use of water based coatings on surfaces greater than 100°C is.. |
|||
Maximum Service Temperature, Inert | 2000 °C | 3630 °F | Vacuum |
Sinotek Materials Rigid Graphite Felt Board Heat Insulation Material Information provided by Sinotek |
|||
Maximum Service Temperature, Inert | 2000 - 3000 °C | 3630 - 5430 °F | Inert/Vacuum Use (BN Component) |
Momentive Performance Materials GPC Boron Nitride (BN) Water Based Coating Solids content > 25%. Can be applied by brush, roller, dipping, or spraying. Can be applied to either hot or cold services although use of water based coatings on surfaces greater than 100°C is n.. |