Thermal Properties | Metric | English | Comments |
---|---|---|---|
Maximum Service Temperature, Inert | 180 °C | 356 °F | |
Haysite EMD Polyester, Glass Reinforced EMD is a glass mat reinforced polyester sheet designed primarily as a "slot wedge" material in large motors and generators. EMD has low weight loss at elevated temperatures and high flexural and sh.. |
|||
Maximum Service Temperature, Inert | 180 °C @Thickness 0.000 mm, Time 7.20e+7 sec |
356 °F @Thickness 0.000 in, Time 20000 hour |
IEC 60216; IEC/EN 60893-2 7.1 |
Elektro-Isola G-Etronax EP 11 Epoxy, Glass Fabric Reinforcement, Green, Sheets Description: High resistance to chemicals. Particularly good, lasting strength properties and insulation values even at high application temperatures. Radiation-resistant. Can be used at cryogenic t.. |
|||
Maximum Service Temperature, Inert | 180 °C @Thickness 3.00 mm, Time 7.20e+7 sec |
356 °F @Thickness 0.118 in, Time 20000 hour |
IEC 60695-11-10; IEC/EN 61212-2 7.1 |
Elektro-Isola G-Etronax EP 11 Epoxy, Glass Fabric Reinforcement, Green, Tubes Description: Particularly good electrical and mechanical properties. Extremely high mechanical strength, even at high temperatures. Retains electrical properties at high air humidity. High resistanc.. |
|||
Maximum Service Temperature, Inert | 180 °C @Thickness 0.000 mm, Time 7.20e+7 sec |
356 °F @Thickness 0.000 in, Time 20000 hour |
IEC 60216; IEC/EN 60893-2 7.1 |
Elektro-Isola G-Etronax EP 215 S Epoxy, Glass Fabric Reinforcement, Green, Sheets Description: Particularly good, lasting strength properties and insulation values even at high application temperatures. Radiation-resistant. Can be used at cryogenic temperatures. Very good where t.. |
|||
Maximum Service Temperature, Inert | 180 °C @Thickness 0.000 mm, Time 7.20e+7 sec |
356 °F @Thickness 0.000 in, Time 20000 hour |
IEC 60216; IEC/EN 60893-2 7.1 |
Elektro-Isola G-Etronax PM H Polyester, Glass Mat, Creme, Sheets Description: A reasonably-priced alternative to other high-temperature types. Low thermal conductivity. Applications: Used as, among other things, thermal insulation plates where high strength prope.. |
|||
Maximum Service Temperature, Inert | 180 °C | 356 °F | |
Arlon 32980X040 0.040" Uncured Silicone Rubber on Polyester Film Design/Construction:Interleave: PolyethyleneSide 1: Uncured Silicone RubberCarrier: Polyester FilmThis data represents typical values for the production material and should not be used as material.. |
|||
Maximum Service Temperature, Inert | 180 °C | 356 °F | |
Arlon 32980X050 0.050" Uncured Silicone Rubber on Polyester Film Design/Construction:Interleave: PolyethyleneSide 1: Uncured Silicone RubberCarrier: Polyester FilmThis data represents typical values for the production material and should not be used as material.. |
|||
Maximum Service Temperature, Inert | 180 °C | 356 °F | |
Arlon 32980X060 0.060" Uncured Silicone Rubber on Polyester Film Design/Construction:Interleave: PolyethyleneSide 1: Uncured Silicone RubberCarrier: Polyester FilmThis data represents typical values for the production material and should not be used as material.. |
|||
Maximum Service Temperature, Inert | 180 °C | 356 °F | |
Arlon 32980X078 0.078" Uncured Silicone Rubber on Polyester Film Design/Construction:Interleave: 3 mil PolyethyleneSide 1: Uncured Silicone RubberCarrier: Polyester FilmThis data represents typical values for the production material and should not be used as ma.. |