Thermal Properties | Metric | English | Comments |
---|---|---|---|
Maximum Service Temperature, Inert | 850 °C | 1560 °F | |
CeramTec ZN 40 Zirconia, ZrO2-MgO ZN 40 is a zirconium oxide ceramic with an excellent surface finish and a higher strength than aluminum oxide. Its good crack resistance and anti-friction properties, combined with steel-like therma.. |
|||
Maximum Service Temperature, Inert | 850 °C | 1560 °F | Non-oxidizing atmosphere |
Sinotek Materials Packing Expanded Graphite Braided Graphite braided packing, made of expanded graphite yarn braids, is resistant to heat, chemicals, and tight sealing. It is widely used in the steam valves of power plants, or as static sealing in pl.. |