Thermal Properties Metric English Comments
Maximum Service Temperature, Inert 1000 °C
1830 °F
CeramTec DC 25 Dispersion Ceramic, Al2O3-ZrO2
DC 25 is a ZTA Alumina Zirconia Platelet Composite used in dental applications.
Maximum Service Temperature, Inert 1000 °C
1830 °F
CeramTec MZ 111 HIP Zirconia, ZrO2-Y2O3
MZ 111 HIP is a yttria-stabilized tetragonal zirconia ceramic.
Maximum Service Temperature, Inert 1000 °C
1830 °F
CeramTec MZ 111 Zirconia, ZrO2-Y2O3
MZ 111 is a yttria-stabilized tetragonal zirconia used in dental applications.
Maximum Service Temperature, Inert 1000 °C
1830 °F
CeramTec MZ 429 Zirconia, ZrO2-Y2O3
MZ 429 is a yttria-stabilized zirconia ceramic.