Thermal Properties Metric English Comments
Thermal Conductivity 110.0 - 140.0 W/m-K
763.4 - 971.6 BTU-in/hr-ft²-°F
ALIMEX 5083 O/H111Aluminum Alloy Rolled
Rolled aluminium material according to DIN EN standard. Information provided by ALIMEX GmbHAnnealed and slightly strain-hardened
Thermal Conductivity 110.0 - 140.0 W/m-K
763.4 - 971.6 BTU-in/hr-ft²-°F
ALIMEX PLANAL 5083 O/H111 Aluminum Alloy
Aluminium rolled plates which have been machined on both sides. Has a precise surface finish and high tensile strength. The temper values and the material conditions are not changed by surface-machi..