Polymer Property : Thermal Conductivity = 96.8 W/m-K Product List

Thermal Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Thermal Properties Metric English Comments
Thermal Conductivity 96.8 W/m-K
672 BTU-in/hr-ft²-°F
Materion BrushCAST® 20C High Strength Casting Alloy (As Cast & Aged)
Pouring Temperature: 1010-1120°CHeat treatment required for max strength (Annealing): 760-790°C/water quenchHeat treatment required for max strength (Hardening): 760-790°C/water quenchDescr..
Thermal Conductivity 96.8 W/m-K
672 BTU-in/hr-ft²-°F
Materion BrushCAST® 20C High Strength Casting Alloy (As Cast)
Pouring Temperature: 1010-1120°CHeat treatment required for max strength (Annealing): 760-790°C/water quenchHeat treatment required for max strength (Hardening): 760-790°C/water quenchDescr..
Thermal Conductivity 96.8 W/m-K
672 BTU-in/hr-ft²-°F
Materion BrushCAST® 20C High Strength Casting Alloy (Solution Annealed & Aged)
Pouring Temperature: 1010-1120°CHeat treatment required for max strength (Annealing): 760-790°C/water quenchHeat treatment required for max strength (Hardening): 760-790°C/water quenchDescr..
Thermal Conductivity 96.8 W/m-K
672 BTU-in/hr-ft²-°F
Materion BrushCAST® 21C High Strength Casting Alloy (As Cast & Aged)
Pouring Temperature: 1010-1120°CHeat treatment required for max strength (Annealing): 760-790°C/water quenchHeat treatment required for max strength (Hardening): 760-790°C/water quenchDescr..
Thermal Conductivity 96.8 W/m-K
672 BTU-in/hr-ft²-°F
Materion BrushCAST® 21C High Strength Casting Alloy (As Cast)
Pouring Temperature: 1010-1120°CHeat treatment required for max strength (Annealing): 760-790°C/water quenchHeat treatment required for max strength (Hardening): 760-790°C/water quenchDescr..
Thermal Conductivity 96.8 W/m-K
672 BTU-in/hr-ft²-°F
Materion BrushCAST® 21C High Strength Casting Alloy (Solution Annealed & Aged)
Pouring Temperature: 1010-1120°CHeat treatment required for max strength (Annealing): 760-790°C/water quenchHeat treatment required for max strength (Hardening): 760-790°C/water quenchDescr..
Thermal Conductivity 96.8 W/m-K
672 BTU-in/hr-ft²-°F
Materion BrushCAST® 20CT Fine Grain Casting Alloy (As Cast & Aged)
Pouring Temperature: 1010-1120°CHeat treatment required for max strength (Annealing): 760-790°C/water quenchHeat treatment required for max strength (Hardening): 760-790°C/water quenchDescr..
Thermal Conductivity 96.8 W/m-K
672 BTU-in/hr-ft²-°F
Materion BrushCAST® 20CT Fine Grain Casting Alloy (As Cast)
Pouring Temperature: 1010-1120°CHeat treatment required for max strength (Annealing): 760-790°C/water quenchHeat treatment required for max strength (Hardening): 760-790°C/water quenchDescr..
Thermal Conductivity 96.8 W/m-K
672 BTU-in/hr-ft²-°F
Materion BrushCAST® 20CT Fine Grain Casting Alloy (Solution Annealed & Aged)
Pouring Temperature: 1010-1120°CHeat treatment required for max strength (Annealing): 760-790°C/water quenchHeat treatment required for max strength (Hardening): 760-790°C/water quenchDescr..