Thermal Properties | Metric | English | Comments |
---|---|---|---|
Thermal Conductivity | 1.40 W/m-K | 9.70 BTU-in/hr-ft²-°F | |
Crucible Steel CSM® S60V (440V) Tool Steel, AISI 440C Modified CPM S60V is a unique tool steel made by the Crucible Particle Metallurgy process. It is designed from a 440C stainless base analysis with added high carbon and vanadium for exceptionally good wear r.. |