Polymer Property : Thermal Conductivity = 80.0 W/m-K Product List

Thermal Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Thermal Properties Metric English Comments
Thermal Conductivity 60.0 - 80.0 W/m-K
416 - 555 BTU-in/hr-ft²-°F
Goodfellow Tungsten Carbide/Cobalt
Tungsten Carbide is a hard, brittle ceramic which, when combined with 6% to 10% Cobalt, forms a tough Cermet (Ceramic-Metal). This material was developed for use in cutting tools, having hard cerami..