Thermal Properties | Metric | English | Comments |
---|---|---|---|
Thermal Conductivity | 0.140 - 1.28 W/m-K | 0.972 - 8.88 BTU-in/hr-ft²-°F | Average value: 0.510 W/m-K Grade Count:28 |
Overview of materials for Epoxy Cure Resin This property data is a summary of similar materials in the MatWeb database for the category "Epoxy Cure Resin". Each property range of values reported is minimum and maximum values of appropriate M.. |
|||
Thermal Conductivity | 0.724 - 1.28 W/m-K | 5.02 - 8.88 BTU-in/hr-ft²-°F | Average value: 1.08 W/m-K Grade Count:6 |
Overview of materials for Epoxy, Cast, Metal Filled This property data is a summary of similar materials in the MatWeb database for the category "Epoxy, Cast, Aluminum Filled". Each property range of values reported is minimum and maximum values of a.. |