Thermal Properties | Metric | English | Comments |
---|---|---|---|
Thermal Conductivity | 8.40 W/m-K | 58.3 BTU-in/hr-ft²-°F | |
Kennametal Stellite Stellite® 33 Completely non-magnetic. Specific Electrical Resistance: 39.8 µOhm/in^3.Applications: standard tool bits, tipped tools, form tools, milling cutter blades, wood working tools, reamer blades, cut-o.. |