Polymer Property : Thermal Conductivity = 74.3 BTU-in/hr-ft²-°F Product List

Thermal Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Thermal Properties Metric English Comments
Thermal Conductivity 10.7 W/m-K

@Temperature 1500 °C
74.3 BTU-in/hr-ft²-°F

@Temperature 2730 °F
Perpendicular
Momentive Performance Materials BNC2 Boron Nitride (BN) Refractory Composite
Boron Nitride is a unique engineering material. It is a soft, machinable ceramic which can be combined with other refractory ceramics including Aluminum Oxide, Silicon Nitride, Aluminum Nitride, Mu..