Polymer Property : Thermal Conductivity = 7.90 W/m-K Product List

Thermal Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Thermal Properties Metric English Comments
Thermal Conductivity 7.90 W/m-K
54.8 BTU-in/hr-ft²-°F
JIS-R-2618; ASTM D2326
Fujipoly Industries Sarcon® GR-Hn Gap Filler Pad
Sarcon GR-n is a highly formable, thermally conductive gel material (no electicity conductive) in a versatile sheet form that easily fits and adheres to most all shapes and sizes of components, and ..
Thermal Conductivity 7.90 W/m-K
54.8 BTU-in/hr-ft²-°F
120°C for 1,000 hrs; JIS-R-2618
Fujipoly Industries Sarcon® GR-Hn Gap Filler Pad
Sarcon GR-n is a highly formable, thermally conductive gel material (no electicity conductive) in a versatile sheet form that easily fits and adheres to most all shapes and sizes of components, and ..
Thermal Conductivity 7.90 W/m-K
54.8 BTU-in/hr-ft²-°F
150°C for 1,000 hrs with 90% RH; JIS-R-2618
Fujipoly Industries Sarcon® GR-Hn Gap Filler Pad
Sarcon GR-n is a highly formable, thermally conductive gel material (no electicity conductive) in a versatile sheet form that easily fits and adheres to most all shapes and sizes of components, and ..
Thermal Conductivity 7.90 W/m-K
54.8 BTU-in/hr-ft²-°F
60°C for 1,000 hrs with 90% RH; JIS-R-2618
Fujipoly Industries Sarcon® GR-Hn Gap Filler Pad
Sarcon GR-n is a highly formable, thermally conductive gel material (no electicity conductive) in a versatile sheet form that easily fits and adheres to most all shapes and sizes of components, and ..
Thermal Conductivity 7.90 W/m-K
54.8 BTU-in/hr-ft²-°F
70°C for 1,000 hrs; JIS-R-2618
Fujipoly Industries Sarcon® GR-Hn Gap Filler Pad
Sarcon GR-n is a highly formable, thermally conductive gel material (no electicity conductive) in a versatile sheet form that easily fits and adheres to most all shapes and sizes of components, and ..
Thermal Conductivity 7.90 W/m-K
54.8 BTU-in/hr-ft²-°F
JIS-R-2618; ASTM D2326
Fujipoly Industries Sarcon® GR-n Gap Filler Pad
Sarcon GR-n is a highly formable, thermally conductive gel material (no electicity conductive) in a versatile sheet form that easily fits and adheres to most all shapes and sizes of components, and ..
Thermal Conductivity 7.90 W/m-K
54.8 BTU-in/hr-ft²-°F
120°C for 1,000 hrs; JIS-R-2618
Fujipoly Industries Sarcon® GR-n Gap Filler Pad
Sarcon GR-n is a highly formable, thermally conductive gel material (no electicity conductive) in a versatile sheet form that easily fits and adheres to most all shapes and sizes of components, and ..
Thermal Conductivity 7.90 W/m-K
54.8 BTU-in/hr-ft²-°F
150°C for 1,000 hrs with 90% RH; JIS-R-2618
Fujipoly Industries Sarcon® GR-n Gap Filler Pad
Sarcon GR-n is a highly formable, thermally conductive gel material (no electicity conductive) in a versatile sheet form that easily fits and adheres to most all shapes and sizes of components, and ..
Thermal Conductivity 7.90 W/m-K
54.8 BTU-in/hr-ft²-°F
60°C for 1,000 hrs with 90% RH; JIS-R-2618
Fujipoly Industries Sarcon® GR-n Gap Filler Pad
Sarcon GR-n is a highly formable, thermally conductive gel material (no electicity conductive) in a versatile sheet form that easily fits and adheres to most all shapes and sizes of components, and ..
Thermal Conductivity 7.90 W/m-K
54.8 BTU-in/hr-ft²-°F
70°C for 1,000 hrs; JIS-R-2618
Fujipoly Industries Sarcon® GR-n Gap Filler Pad
Sarcon GR-n is a highly formable, thermally conductive gel material (no electicity conductive) in a versatile sheet form that easily fits and adheres to most all shapes and sizes of components, and ..