Thermal Properties | Metric | English | Comments |
---|---|---|---|
Thermal Conductivity | 1.13 W/m-K @Temperature 166 °C |
7.84 BTU-in/hr-ft²-°F @Temperature 331 °F |
|
Schott AF 45 Thin Borosilicate Glass AF 45 is an alkali-free modified borosilicate glass with a high content of BaO and Al2O3. AF 45 with, its specific properties and large range of different thicknesses with tight tolerances, is exc.. |