Thermal Properties | Metric | English | Comments |
---|---|---|---|
Thermal Conductivity | 67.1 W/m-K @Temperature 100 °C |
466 BTU-in/hr-ft²-°F @Temperature 212 °F |
|
ATI Allegheny Ludlum AL 200™ Nickel Alloy, UNS N02200 Ferromagnetic. Allegheny Ludlum AL 200 alloy is wrought commercially pure nickel. This alloy provides highly ductile mechanical properties across a wide temperature range. Either alloy provides c.. |
|||
Thermal Conductivity | 67.1 W/m-K @Temperature 100 °C |
466 BTU-in/hr-ft²-°F @Temperature 212 °F |
|
ATI Allegheny Ludlum AL 201™ Nickel Alloy, UNS N02201 Ferromagnetic. Allegheny Ludlum AL 201 alloy is wrought commercially pure nickel. This alloy provides highly ductile mechanical properties across a wide temperature range. Either alloy provides c.. |