Thermal Properties Metric English Comments
Thermal Conductivity 63.0 - 155 W/m-K

@Temperature 20.0 °C
437 - 1080 BTU-in/hr-ft²-°F

@Temperature 68.0 °F
Acerde Silicon Carbide
Silicon Carbide key properties: High oxidation resistance, High hardness, Resistive to thermal stress, High thermal conductivity, Low thermal expansion, High elastic modulus, Superior chemical inert..