Thermal Properties | Metric | English | Comments |
---|---|---|---|
Thermal Conductivity | 62.0 W/m-K | 430 BTU-in/hr-ft²-°F | |
Parkway Products Thixomolded® AM50A Magnesium Thixomolding® is a fabrication technique, similar to injection molding, that uses magnesium alloys as the “resin” instead of plastic. Solid magnesium alloy pellets are fed into the machine, heate.. |
|||
Thermal Conductivity | 62.0 W/m-K | 430 BTU-in/hr-ft²-°F | |
Parkway Products Thixomolded® AM60A Magnesium Thixomolding® is a fabrication technique, similar to injection molding, that uses magnesium alloys as the “resin” instead of plastic. Solid magnesium alloy pellets are fed into the machine, heate.. |