Thermal Properties Metric English Comments
Thermal Conductivity 86.5 W/m-K
600 BTU-in/hr-ft²-°F
Chicago Extruded Metals BioBrass® UNS C62300 Aluminum Bronze
Finished product available as bar, rod, forged or shapes.Chicago Extruded Metal temper codes: H02, M30This alloy is registered with the U.S. EPA as Antimicrobial.Information provided by Chicago Extr..
Thermal Conductivity 86.5 W/m-K
600 BTU-in/hr-ft²-°F
Chicago Extruded Metals BioBrass® UNS C62400 Aluminum Bronze
Finished product available as rod or forged.Chicago Extruded Metal temper codes: H02, M30This alloy is registered with the U.S. EPA as Antimicrobial.Information provided by Chicago Extruded Metals