Thermal Properties Metric English Comments
Thermal Conductivity 0.890 W/m-K
6.18 BTU-in/hr-ft²-°F
Epoxy Technology EPO-TEK® H31D-LV Epoxy
Material Description: A single component, silver-filled, electrically conductive epoxy designed for semiconductor die attach applications found in hybrids, JEDEC, and optoelectronic packaging. It i..