Thermal Properties | Metric | English | Comments |
---|---|---|---|
Thermal Conductivity | 0.8724 W/m-K @Temperature 1000 °C |
6.044 BTU-in/hr-ft²-°F @Temperature 1830 °F |
|
Chosun Refractories INCT-170 Light-Weight Castable Information provided by Chosun Refractories via Korea Institute of Ceramic Engineering and Technology (KICET). |