Thermal Properties | Metric | English | Comments |
---|---|---|---|
Thermal Conductivity | 59.8 W/m-K @Temperature 27.0 °C |
415 BTU-in/hr-ft²-°F @Temperature 80.6 °F |
|
Mateck Germanium (Ge) Optical crystals |