Polymer Property : Thermal Conductivity = 59.0 BTU-in/hr-ft²-°F Product List

Thermal Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Thermal Properties Metric English Comments
Thermal Conductivity 8.50 W/m-K
59.0 BTU-in/hr-ft²-°F
Cytec Thornel® T-300 12K Carbon Fiber, Polyacrylonitrile (PAN) Precursor
Data provided by the manufacturer, Amoco Performance Products, Inc.Continuous length, high strength, high modulus fiber made from a polyacrylonitrile precursor. The fiber surface has been treated t..
Thermal Conductivity 8.50 W/m-K
59.0 BTU-in/hr-ft²-°F
Cytec Thornel® T-300 1K Carbon Fiber, Polyacrylonitrile (PAN) Precursor
Data provided by the manufacturer, Amoco Performance Products, Inc.Continuous length, high strength, high modulus fiber made from a polyacrylonitrile precursor. The fiber surface has been treated t..
Thermal Conductivity 8.50 W/m-K
59.0 BTU-in/hr-ft²-°F
Cytec Thornel® T-300 3K Carbon Fiber, Polyacrylonitrile (PAN) Precursor
Data provided by the manufacturer, Amoco Performance Products, Inc.Continuous length, high strength, high modulus fiber made from a polyacrylonitrile precursor. The fiber surface has been treated t..
Thermal Conductivity 8.50 W/m-K
59.0 BTU-in/hr-ft²-°F
Cytec Thornel® T-300 6K Carbon Fiber, Polyacrylonitrile (PAN) Precursor
Data provided by the manufacturer, Amoco Performance Products, Inc.Continuous length, high strength, high modulus fiber made from a polyacrylonitrile precursor. The fiber surface has been treated t..