Thermal Properties | Metric | English | Comments |
---|---|---|---|
Thermal Conductivity | 0.303 - 8.00 W/m-K | 2.10 - 55.5 BTU-in/hr-ft²-°F | Average value: 2.00 W/m-K Grade Count:13 |
Overview of materials for Polyphenylene Sulfide (PPS) with 10% Glass Fiber Filler This property data is a summary of similar materials in the MatWeb database for the category "Polyphenylene Sulfide (PPS) with 10% Glass Fiber Filler". Specific grades with glass content between 5% .. |