Thermal Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Thermal Properties Metric English Comments
Thermal Conductivity 54.0 W/m-K

@Temperature 85.0 °C
375 BTU-in/hr-ft²-°F

@Temperature 185 °F
Indium Corp. Indalloy® 227 Sn-In-Ag Solder Alloy
Pb free solder can be used as a replacement for 63Sn 37Pb, 62Sn 36Pb 2Ag and 60Sn 40Pb in that it has similar physical and mechanical properties. Not for use over 100°C due to 118°C Sn/In eut..
Thermal Conductivity 54.0 W/m-K
375 BTU-in/hr-ft²-°F
Williams Advanced Alloys WS187 Solder
All Williams alloys are available in a variety of shapes and forms, including ribbon, preforms, rod, ring, wire, and custom shapes.Information provided by Williams Advanced Alloys