Thermal Properties Metric English Comments
Thermal Conductivity 53.329 W/m-K
370.08 BTU-in/hr-ft²-°F
Dura-Bar G2 Continuously Cast Gray Iron Bar Stock ASTM A48
Continuously cast ductile iron bar stock is produced in a wide variety of sizes and shapes, including rounds, rectangles and special shape cross sections.It often is used as an alternative to gray i..