Thermal Properties | Metric | English | Comments |
---|---|---|---|
Thermal Conductivity | 0.851 W/m-K | 5.91 BTU-in/hr-ft²-°F | |
Schott N-SK14 Glass Information Provided by SCHOTT North America, Inc. |
|||
Thermal Conductivity | 0.854 W/m-K | 5.91 BTU-in/hr-ft²-°F | ASTM C177 |
Devcon Fastmeal™ Epoxy Precision Repair EpoxyComments: High-performance, alumina-filled epoxy putty for making fast, dependable emergency repair to leaks in pipes carrying ores, coal, cement, san and gravel. Cures in 5 m.. |