Thermal Properties | Metric | English | Comments |
---|---|---|---|
Thermal Conductivity | 5.90 W/m-K | 40.9 BTU-in/hr-ft²-°F | DIN EN 821-2 / ASTM-C408 |
CeramTec 665 Steatite, MgO•SiO2 Steatites used in place of aluminas are a cost-effective way to meet performance requirements. They are easier to form and fire at lower temperatures. 665 L533C has low dielectric loss. It makes exc.. |