Thermal Properties | Metric | English | Comments |
---|---|---|---|
Thermal Conductivity | >= 0.793 W/m-K | >= 5.50 BTU-in/hr-ft²-°F | ASTM C177 |
PolyOne Edgetek® AM-30CF/000 Polyphthalamide (PPA), Carbon Fiber Reinforced
(discontinued **) Description/Features:Carbon Fiber ReinforcedPolyOne First ChoiceInformation provided by PolyOne Corporation. |