Thermal Properties | Metric | English | Comments |
---|---|---|---|
Thermal Conductivity | 49.0 W/m-K @Temperature 85.0 °C |
340 BTU-in/hr-ft²-°F @Temperature 185 °F |
|
Indium Corp. Indalloy 109 Tin-Lead Solder Alloy Good electrical grade solderInformation Provided by Indium Corporation |
|||
Thermal Conductivity | 49.0 W/m-K @Temperature 85.0 °C |
340 BTU-in/hr-ft²-°F @Temperature 185 °F |
|
Indium Corp. Indalloy 259 Tin Solder Alloy Information Provided by Indium Corporation |
|||
Thermal Conductivity | 49.0 W/m-K | 340 BTU-in/hr-ft²-°F | |
Williams Advanced Alloys WS188 Solder All Williams alloys are available in a variety of shapes and forms, including ribbon, preforms, rod, ring, wire, and custom shapes.Information provided by Williams Advanced Alloys |