Polymer Property : Thermal Conductivity = 46.8 W/m-K Product List

Thermal Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Thermal Properties Metric English Comments
Thermal Conductivity 46.8 W/m-K

@Temperature 10.0 - 232 °C
325 BTU-in/hr-ft²-°F

@Temperature 50.0 - 450 °F
Meehanite GC-40 Flake Graphite Cast Iron
Type GC-40 combines good strength with low coefficient of friction and self lubricating properties. It is easily machinable with a fine, dense, close grain structure. Recommended for heavy brake d..