Thermal Properties | Metric | English | Comments |
---|---|---|---|
Thermal Conductivity | 640 W/m-K | 4440 BTU-in/hr-ft²-°F | |
Cytec Thornel® P-120 2K Carbon Fiber, Pitch Precursor Data provided by the manufacturer, Amoco Performance Products, Inc.Continuous filament, ultra high modulus fibers consisting of 2000 filaments in a one-ply construction.2000 filaments/strand, 0.33 m.. |
|||
Thermal Conductivity | 640 W/m-K | 4440 BTU-in/hr-ft²-°F | |
Cytec Thornel® P-120S 2K Carbon Fiber, Pitch Precursor Data provided by the manufacturer, Amoco Performance Products, Inc.Continuous filament, ultra high modulus fibers consisting of 2000 filaments in a one-ply construction. The fiber surface has been .. |