Thermal Properties | Metric | English | Comments |
---|---|---|---|
Thermal Conductivity | 43.2 W/m-K @Temperature 15.6 °C |
300 BTU-in/hr-ft²-°F @Temperature 60.0 °F |
|
Performance Alloys MoldStar® 21 (PAS 21) Bronze Mold Alloy Description: MoldStar® 21 bronze alloy provides good bearing qualities and resistance to wear, abrasion, fatigue, deformation and corrosion.Applications: Lifter BladesSlidesGibsWear PlatesEjector S.. |
|||
Thermal Conductivity | 43.2 W/m-K @Temperature 15.6 °C |
300 BTU-in/hr-ft²-°F @Temperature 60.0 °F |
|
Performance Alloys MoldStar® 22 (PAS 22) Bronze Mold Alloy Description: MoldStar® 21 bronze alloy provides good bearing qualities and resistance to wear, abrasion, fatigue, deformation and corrosion.Applications: Ejector SleevesLifter BladesThin Wall Appli.. |