Thermal Conductivity 57.7 W/m-K
400 BTU-in/hr-ft²-°F
California Fine Wire Permanickel® K-300 Nickel Alloy
All values may vary dependent on specific design and usagePermanickel® is a registered trade name of the Inco family of products.Capabilities: WireRibbonInsulatedPlatedInformation provided by Calif..