Thermal Properties | Metric | English | Comments |
---|---|---|---|
Thermal Conductivity | 40.1 W/m-K @Temperature 10.0 - 232 °C |
278 BTU-in/hr-ft²-°F @Temperature 50.0 - 450 °F |
|
Meehanite HSV Heat Resisting Cast Iron Type HSV is an iron developed essentially for engineering parts subjected to long continuous heating. It has been designed to have the maximum load bearing ability.General Meehanite information - M.. |