Thermal Properties Metric English Comments
Thermal Conductivity 0.649 W/m-K
4.49 BTU-in/hr-ft²-°F
Cytec EN-2552 (Conap) Potting and Encapsulation Adhesive
Polyurethane Potting and Encapsulating SystemsConathane® EN-2500 series polyurethane potting and encapsulating systems from Cytek have varying degrees of worklife, viscosity and hardness for many s..
Thermal Conductivity 0.649 W/m-K
4.49 BTU-in/hr-ft²-°F
Cytec EN-2551 (Conap) Potting and Encapsulation Adhesive
Polyurethane Potting and Encapsulating SystemsConathane® EN-2500 series polyurethane potting and encapsulating systems from Cytek have varying degrees of worklife, viscosity and hardness for many s..