Thermal Properties | Metric | English | Comments |
---|---|---|---|
Thermal Conductivity | 57.0 W/m-K @Temperature 85.0 °C |
396 BTU-in/hr-ft²-°F @Temperature 185 °F |
|
Indium Corp. Indalloy® 182 Au-Sn Solder Alloy Eutectic die attach and package sealing.Information provided by the manufacturer, Indium Corporation. |
|||
Thermal Conductivity | 57.0 W/m-K | 396 BTU-in/hr-ft²-°F | |
Williams Advanced Alloys WS280B Solder (Au80/Sn20) All Williams alloys are available in a variety of shapes and forms, including ribbon, preforms, rod, ring, wire, and custom shapes.Information provided by Williams Advanced Alloys |
|||
Thermal Conductivity | 57.0 W/m-K | 396 BTU-in/hr-ft²-°F | |
Williams Advanced Alloys WS305 Solder All Williams alloys are available in a variety of shapes and forms, including ribbon, preforms, rod, ring, wire, and custom shapes.Information provided by Williams Advanced Alloys |