Thermal Conductivity 36.7 W/m-K

@Temperature 1200 °C
255 BTU-in/hr-ft²-°F

@Temperature 2190 °F
Haynes 214® alloy sheet
Intended principally for use at temperatures of 955°C and above, exhibits resistance to oxidation that exceeds virtually all conventional heat-resistant wrought alloys. Applications include mesh ..
Thermal Conductivity 36.7 W/m-K

@Temperature 1200 °C
255 BTU-in/hr-ft²-°F

@Temperature 2190 °F
Haynes 214® alloy, sheet, 100 hours exposure at 760°C (1400°F)
Intended principally for use at temperatures of 955°C and above, exhibits resistance to oxidation that exceeds virtually all conventional heat-resistant wrought alloys. Applications include mesh ..
Thermal Conductivity 36.7 W/m-K

@Temperature 1200 °C
255 BTU-in/hr-ft²-°F

@Temperature 2190 °F
Haynes 214® alloy, sheet, 100 hours exposure at 870°C (1600°F)
Intended principally for use at temperatures of 955°C and above, exhibits resistance to oxidation that exceeds virtually all conventional heat-resistant wrought alloys. Applications include mesh ..
Thermal Conductivity 36.7 W/m-K

@Temperature 1200 °C
255 BTU-in/hr-ft²-°F

@Temperature 2190 °F
Haynes 214® alloy, sheet, 100 hours exposure at 980°C (1800°F)
Intended principally for use at temperatures of 955°C and above, exhibits resistance to oxidation that exceeds virtually all conventional heat-resistant wrought alloys. Applications include mesh ..
Thermal Conductivity 36.7 W/m-K

@Temperature 1200 °C
255 BTU-in/hr-ft²-°F

@Temperature 2190 °F
Haynes 214® alloy, sheet, 1000 hours exposure at 760°C (1400°F)
Intended principally for use at temperatures of 955°C and above, exhibits resistance to oxidation that exceeds virtually all conventional heat-resistant wrought alloys. Applications include mesh ..
Thermal Conductivity 36.7 W/m-K

@Temperature 1200 °C
255 BTU-in/hr-ft²-°F

@Temperature 2190 °F
Haynes 214® alloy, sheet, 1000 hours exposure at 870°C (1600°F)
Intended principally for use at temperatures of 955°C and above, exhibits resistance to oxidation that exceeds virtually all conventional heat-resistant wrought alloys. Applications include mesh ..
Thermal Conductivity 36.7 W/m-K

@Temperature 1200 °C
255 BTU-in/hr-ft²-°F

@Temperature 2190 °F
Haynes 214® alloy, sheet, 1000 hours exposure at 980°C (1800°F)
Intended principally for use at temperatures of 955°C and above, exhibits resistance to oxidation that exceeds virtually all conventional heat-resistant wrought alloys. Applications include mesh ..
Thermal Conductivity 36.7 W/m-K

@Temperature 1200 °C
255 BTU-in/hr-ft²-°F

@Temperature 2190 °F
Haynes 214® alloy, sheet, 32 hours exposure at 760°C (1400°F)
Intended principally for use at temperatures of 955°C and above, exhibits resistance to oxidation that exceeds virtually all conventional heat-resistant wrought alloys. Applications include mesh ..
Thermal Conductivity 36.7 W/m-K

@Temperature 1200 °C
255 BTU-in/hr-ft²-°F

@Temperature 2190 °F
Haynes 214® alloy, sheet, 32 hours exposure at 870°C (1600°F)
Intended principally for use at temperatures of 955°C and above, exhibits resistance to oxidation that exceeds virtually all conventional heat-resistant wrought alloys. Applications include mesh ..
Thermal Conductivity 36.7 W/m-K

@Temperature 1200 °C
255 BTU-in/hr-ft²-°F

@Temperature 2190 °F
Haynes 214® alloy, sheet, 32 hours exposure at 980°C (1800°F)
Intended principally for use at temperatures of 955°C and above, exhibits resistance to oxidation that exceeds virtually all conventional heat-resistant wrought alloys. Applications include mesh ..