Polymer Property : Thermal Conductivity = 347.6 W/m-K Product List

Thermal Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Thermal Properties Metric English Comments
Thermal Conductivity 347.6 W/m-K
2412 BTU-in/hr-ft²-°F
Eagle Brass 19210 XP-10 Copper Iron, 1/2 Hard
19210 has higher strengths than most copper alloys but thanks to its composition and processing it retains formability and conductivity that other copper alloys lose. Typical uses include cooling f..
Thermal Conductivity 347.6 W/m-K
2412 BTU-in/hr-ft²-°F
Eagle Brass 19210 XP-10 Copper Iron, 1/4 Hard
19210 has higher strengths than most copper alloys but thanks to its composition and processing it retains formability and conductivity that other copper alloys lose. Typical uses include cooling f..
Thermal Conductivity 347.6 W/m-K
2412 BTU-in/hr-ft²-°F
Eagle Brass 19210 XP-10 Copper Iron, 3/4 Hard
19210 has higher strengths than most copper alloys but thanks to its composition and processing it retains formability and conductivity that other copper alloys lose. Typical uses include cooling f..
Thermal Conductivity 347.6 W/m-K
2412 BTU-in/hr-ft²-°F
Eagle Brass 19210 XP-10 Copper Iron, Annealed
19210 has higher strengths than most copper alloys but thanks to its composition and processing it retains formability and conductivity that other copper alloys lose. Typical uses include cooling f..
Thermal Conductivity 347.6 W/m-K
2412 BTU-in/hr-ft²-°F
Eagle Brass 19210 XP-10 Copper Iron, Extra Hard
19210 has higher strengths than most copper alloys but thanks to its composition and processing it retains formability and conductivity that other copper alloys lose. Typical uses include cooling f..
Thermal Conductivity 347.6 W/m-K
2412 BTU-in/hr-ft²-°F
Eagle Brass 19210 XP-10 Copper Iron, Extra Spring
19210 has higher strengths than most copper alloys but thanks to its composition and processing it retains formability and conductivity that other copper alloys lose. Typical uses include cooling f..
Thermal Conductivity 347.6 W/m-K
2412 BTU-in/hr-ft²-°F
Eagle Brass 19210 XP-10 Copper Iron, Hard
19210 has higher strengths than most copper alloys but thanks to its composition and processing it retains formability and conductivity that other copper alloys lose. Typical uses include cooling f..
Thermal Conductivity 347.6 W/m-K
2412 BTU-in/hr-ft²-°F
Eagle Brass 19210 XP-10 Copper Iron, Spring
19210 has higher strengths than most copper alloys but thanks to its composition and processing it retains formability and conductivity that other copper alloys lose. Typical uses include cooling f..