Thermal Properties | Metric | English | Comments |
---|---|---|---|
Thermal Conductivity | 456.5 W/m-K | 3168 BTU-in/hr-ft²-°F | |
Eagle Brass 18665 MSP1, 1/2 Hard MSP-1 high performance copper alloy with magnesium has high conductivity (63% IACS), high strength and excellent thermal creep properties. Typical uses include terminals, connectors, relays, springs.. |
|||
Thermal Conductivity | 456.5 W/m-K | 3168 BTU-in/hr-ft²-°F | |
Eagle Brass 18665 MSP1, 1/4 Hard MSP-1 high performance copper alloy with magnesium has high conductivity (63% IACS), high strength and excellent thermal creep properties. Typical uses include terminals, connectors, relays, springs.. |
|||
Thermal Conductivity | 456.5 W/m-K | 3168 BTU-in/hr-ft²-°F | |
Eagle Brass 18665 MSP1, Annealed MSP-1 high performance copper alloy with magnesium has high conductivity (63% IACS), high strength and excellent thermal creep properties. Typical uses include terminals, connectors, relays, springs.. |
|||
Thermal Conductivity | 456.5 W/m-K | 3168 BTU-in/hr-ft²-°F | |
Eagle Brass 18665 MSP1, Extra Hard MSP-1 high performance copper alloy with magnesium has high conductivity (63% IACS), high strength and excellent thermal creep properties. Typical uses include terminals, connectors, relays, springs.. |
|||
Thermal Conductivity | 456.5 W/m-K | 3168 BTU-in/hr-ft²-°F | |
Eagle Brass 18665 MSP1, Hard MSP-1 high performance copper alloy with magnesium has high conductivity (63% IACS), high strength and excellent thermal creep properties. Typical uses include terminals, connectors, relays, springs.. |
|||
Thermal Conductivity | 456.5 W/m-K | 3168 BTU-in/hr-ft²-°F | |
Eagle Brass 18665 MSP1, Spring MSP-1 high performance copper alloy with magnesium has high conductivity (63% IACS), high strength and excellent thermal creep properties. Typical uses include terminals, connectors, relays, springs.. |