Thermal Properties Metric English Comments
Thermal Conductivity 300 - 310 W/m-K
2080 - 2150 BTU-in/hr-ft²-°F
x-y direction
MarkeTech Cu/Mo/Cu 1:1:1 Laminated Sheet
Cu/MoCu sheets have very high in-plane thermal conductivity provide by layers of Cu and low CTEs provided by the inner layer of molybdenum. These laminated sheets spread heat from a concentrated hea..