Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Polymer Property : Thermal Conductivity = 3.97 BTU-in/hr-ft²-°F Product List

Thermal Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Thermal Properties Metric English Comments
Thermal Conductivity 0.573 W/m-K
3.97 BTU-in/hr-ft²-°F
ASTM C177
ITW Devcon Plastic Steel® Metal Repair (A), Dark Grey
Information provided by ITW Devcon
Thermal Conductivity 0.573 W/m-K
3.97 BTU-in/hr-ft²-°F
ASTM C177
Devcon Plastic Steel® Putty (A) Epoxy
General Repair EpoxyComments: The original metal-filled epoxy putty used for hundreds of routine maintenance, production and tooling applications. Bonds to most metal, concrete and some plastics. ..
Copyright © lookpolymers.com All Rights Reserved